五流大方坯中间包控流装置优化的数值和物理模拟
罗荣华, 倪红卫, 张华, 赵中福, 陈迪庆
Numerical and Physical Simulation on Optimization of Flow Control Devices in Tundish for Five-Strand Bloom Casting
Luo Ronghua , Ni Hongwei , Zhang Hua , Zhao Zhongfu , Chen Diqing
特殊钢
.
2012, (4): 13
-17
.