12流小方坯6流中间包结构优化的数值模拟和冶金效果
韩传基, 安航航, 季维, 李富帅, 陶金明, 王剑峰, 贾建平
Numerical Simulation and Metallurgical Effect for Structure Optimization of 6-Strand Tundish for 12-Strand Casting Billets
Han Chuanji , An Hanghang , Ji Wei' , Li Fushuai , Tao Jinming , Wang Jianfeng , Jia Jianping
特殊钢
.
2011, (4): 14
-17
.