高碳铬轴承钢碳化物带状评定方法探究
张林, 刘海, 官跃辉, 蒋楠, 陆长河, 张剑锋
Research on Evaluation Method of Carbide Band in High Carbon Chromium Bearing Steel
Zhang Lin, Liu Hai, Guan Yuehui, Jiang Nan, Lu Changhe, Zhang Jianfeng
特殊钢
.
2022, (6): 42
-45
.
DOI: 10.20057/j.1003-8620.2022-00092