圆坯连铸GCr15SiMn的成分偏析和接触疲劳寿命研究
俞峰, 陈兴品, 杜松林, 王存宇, 汪开忠, 曹文全
Composition Segregation and Contact Fatigue Life of GCr15SiMn Fabricated by Round Billet Continuous Casting
Yu Feng, Chen Xingpin, Du Songlin, Wang Cunyu, Wang Kaizhong, Cao Wenquan
特殊钢
.
2022, (6): 13
-20
.
DOI: 10.20057/j.1003-8620.2022-00160