低碳超高强度Q & P钢板的热处理工艺和组织性能
董 辰, 江海涛, 陈雨来, 唐 获, 程知松
Heat Treatment Process and Structure of a Low Carbon Super-high Strength Quenching and Partitioning Steel Plate
Dong Chen , Jiang Haitao , Chen Yulai , Tang Di , Cheng Zhisong
特殊钢
.
2009, (5): 68
-70
.