Inconel 690镍基合金平衡相的热力学计算和实验分析
丰涵, 宋志刚, 郑文杰, 陈斌, 季祥民, 郭志鹏
Thermodynamic Calculation and Experimental Analysis on Equilibrium Phases in Nickel Base Alloy Inconel 690
Feng Han, Song Zhigang, Zheng Wenjie, Chen Bin, Ji Xiangmin , Guo Zhipeng
特殊钢
.
2008, (4): 13
-15
.