冷拔变形量对30CrMnSiNi2A六角材晶粒度及脱碳判定的影响
赵成志, 张玉春, 李建新, 庞学东, 孙勇, 翟羽佳, 梁晓东
Effect of Cold Drawing Deformation on Grain Size and Decarbonization Determination of 30CrMnSiNi2A Hexagonal Products
Zhao Chengzhi, Zhang Yuchun, Li Jianxin, Pang Xuedong, Sun Yong, ZhaiYujia , Liang Xiaodong
特殊钢
.
2023, (3): 109
-113
.
DOI: 10.20057/j.1003-8620.2022-00159