重钢5流方坯连铸中间包控流装置的数理研究
陈登福, 佐祥均, 郑 辉, 黄 丽, 龙木军, 廖 明, 周远华
Physical and Mathematical Study on Flow Control Device of Tundish for 5-Strand billet Casting at Chongqing Steel
Chen Dengfu, Zuo Xiangjun, Zheng Hu i, Huang Li, Long Mujun, Liao Ming, Zhou Yuanhua
特殊钢
.
2007, (1): 1
-3
.