445J2超纯铁素体不锈钢和316L超低碳奥氏体不锈钢在溴化锂溶液的点蚀分析
武卓杰, 侯利锋, 杜华云, 邹 勇, 武敏, 范光伟, 卫英慧
Pitting Erosion Analysis of Ultra-Pure Ferritic Stainless Steel 445J2 and 316L Ultra-Low-Carbon Austenitic Stainless Steel in Lithium Bromide Solution
Wu Zhuojie, Hou Lifeng, Du Huayun, Zou Yong, WuMin, Fan Guangwei, Wei Yinghui,
特殊钢
.
2023, (1): 65
-71
.
DOI: 10.20057/j.1003-8620.2022-00069