轧制工艺对高强度车轮AG650LW轮辋钢的组织和性能的影响
万国喜, 刘艳红, 刘 鹏, 何晓波
Effect of Rolling Process on Structure and Properties of Wheel Rim Steel AG650LW for High Strength Wheel
Wan Guoxi, Liu Yanhong, Liu Peng, He Xiaobo
特殊钢
.
2023, (1): 83
-88
.
DOI: 10.20057/j.1003-8620.2022-00031