K-OBM-S转炉冶炼不锈钢过程的数学模拟和应用
董艳伍, 姜周华, 龚伟, 李建民, 尝天印, 王彦明, 刘卫东
Mathematical Modeling of K-OBM-S Converter Melting Process for Steelmaking of Stainless Steel
Dong Yanwu , Jiang Zhouhua , Gong Wei , Li Jianmin , Chang Tianyin , Wang Yanming , Liu Weidong
特殊钢
.
2006, (2): 13
-16
.