长水口氩封保护浇铸对车轮钢Φ450 mm 圆坯质量的影响
吴宗双, 包 燕 平, 刘 建 华, 陈 刚, 龚 志 翔, 钟 斌
Effect of Long Nozzle Casting with Shielding Argon Gas on Quality of Φ450 mm Round Billet of Wheel Steel
Wu Zongshuang, Bao Yanping, Liu Jianhua, Chen Gang, Gong Zhixiang, Zhong Bin
特殊钢
.
2007, (2): 54
-55
.