B₂O₃ 对 CaO-Al₂O₃-SiO₂-MgO-CaF₂ 五元精炼渣系熔化特性的影响
于学斌, 时启龙, 翟荣灿, 朱志强, 程 亮, 栾启川
Influence of B₂O₃ on Melting Characteristics of CaO-Al₂O₃-SiO₂-MgO-CaF₂ Pentary Slag Series
Yu Xuebin, Shi Qilong, Zhai Rongcan, Zhu Zhiqiang, Cheng Liang, Luan Qichuan
特殊钢
.
2006, (4): 5
-7
.