热轧板常化温度对冷轧无取向电工钢退火组织和磁性能的影响
菅瑞雄. 张文康. 杜振民, 毛卫民, 王一德
Effect of Normalizing Temperature on Structure and Magnetic Properties of Annealed Non-Oriented Electric Steel
Jian Ruixiong, Zhang Wenkang, Du Zhengnin, Mao Weimin, Wang Yide
特殊钢
.
2006, (4): 31
-33
.