石油钻铤用4145H热轧圆钢用Φ600 mm圆坯加热装炉优化
张新文, 轩康乐, 孟祥岩, 施嘉凯, 刘永
Heating Furnace Charging Optimization of Hot Rolled Round Billet 4145H Φ600 mm for Petroleum Drill Collars
Zhang Xinwen, Xuan Kangle, Meng Xiangyan, Shi Jiakai, Liu Yong
特殊钢
.
2023, (3): 94
-97
.
DOI: 10.20057/j.1003-8620.2022-00222