Φ800 mm圆坯Q355NE凝固传热数值模拟和工艺实践
周伟基, 姚玉东, 刘佳伟, 岳峰, 张磊
Numerical Simulation and Process Practice for Solidification and Heat Transfer of Φ800 mm Round Billet Q355NE
Zhou Weiji , Yao Yudong , Liu Jiawei , Yue Feng , Zhang Lei
特殊钢
.
2023, (2): 7
-11
.
DOI: 10.20057/j.1003-8620.2022-00132