20CrH温锻内星齿轮混晶原因分析及工艺改进
徐乐钱, 左锦中, 袁静, 莫秉干, 吴 炜
Analysis and Process Improvement of Mixed Crystal in Warm Forged 20CrH Inner Star Wheel
Xu Leqian , Zuo Jinzhong , Yuan Jing , Mo Binggan , Wu Wei
特殊钢
.
2023, (2): 21
-24
.
DOI: 10.20057/j.1003-8620.2022-00148