冷却速率对新型C61齿轮钢力学性能和微观组织的影响
齐明, 梁晓东, 韩大虹, 任建民, 张智超, 王旭
Effect of Cooling Rate on Mechanical Properties and Microstructure of New C61 Gear Steel
Qi Ming , Liang Xiaodong , Han Dahong , Ren Jianmin , Zhang Zhichao , Wang Xu
特殊钢
.
2023, (2): 80
-83
.
DOI: 10.20057/j.1003-8620.2022-00106