70 t 电弧炉炼钢集束射流氧枪流场的数值模拟及应用
张 贵, 朱 荣, 韩丽辉, 朱长富, 谈知良, 刘长春
Numerical Simulation on Oxygen Stream Field of Coherent Jet Oxygen Lance and Application to a 70 t Arc Furnace
Zhang Gui, Zhu Rong, Han Lihui, Zhu Changfu, Tan Zhiliang, Liu Changchun
特殊钢
.
2006, (5): 46
-48
.