Φ300 mm S53 马氏体时效强化钢环状花样低倍组织分析及工艺改进
董晓亮, 张秀丽, 许广鹏, 阮 栋, 费三林, 曹 广, 廖 凯
Analysis on Ring Pattern Macrostructure of Φ300 mm S53 Ageing
Strengthening Martensitic Steel and Process Improvement
Dong Xiaoliang, Zhang Xiuli, Xu Guangpeng, Ruan Dong, Fei Sanlin, Cao Guang, Liao Kai
特殊钢
.
2022, (1): 69
-72
.