甲醇合成塔用 150 mm SA387Gr22C12 钢板组织和力学性能
尹卫江, 李 杰, 吴艳阳, 王甜甜, 张 剑, 侯敬超
Microstructure and Mechanical Properties of 150 mm
SA387Gr22C12 Steel Plate for Methanol Synthesis Tower
Yin Weijiang, Li Jie, Wu Yanyang, Wang Tiantian, Zhang Jian, Hou Jingchao
特殊钢
.
2022, (1): 93
-96
.