冷轧变形量对高氮奥氏体不锈钢Mn17Cr19N0.6组织和性能的影响
李建新, 赵英利, 王国营, 嵇爽, 陈文, 白丽娟, 裴建明
Effect of Cold Rolling Deformation on Structure and Property of High Nitrogen Austenitic Stainless Steel Mn17Cr19N0.6
Li Jianxin , Zhao Yingli, Wan Guoying, Ji Shuang , Chen Wen , Bai Lijuan , Pei Jianming
特殊钢
.
2020, (1): 61
-63
.