电渣重熔渣系对C-HRA-3耐热合金夹杂物的影响
李龙飞, 林腾昌, 张强, 何西扣, 陈正宗, 周晓舟
The Effect of Electroslag Remelting Slag System on Inclusions in C-HRA-3 Heat-Resistant Alloy
Li Longfei, Lin Tengchang, Zhang Qiang, He Xikou, Chen Zhengzong , Zhou Xiaozhou
特殊钢
.
2023, (5): 76
-82
.
DOI: 10.20057/j.1003-8620.2023-00089