120 t复吹转炉高拉碳低磷出钢的冶炼工艺改进
张福东, 武波, 王月聪, 赵欣, 梁超
The Smelting Process Improvement of 120 t Top-Bottom Combined Blown Converter with High-Carbon Turndown and Low Phosphorus Tapping
Zhang Fudong, Wu Bo, Wang Yuecong, Zhao Xin, Liang Chao
特殊钢
.
2023, (6): 63
-69
.
DOI: 10.20057/j.1003-8620.2023-00049