S44535铁素体不锈钢高温氧化行为
曹小强, 贾建文, 岳习文, 胡群昆, 卫英慧, 侯利锋
High Temperature Oxidation Behavior of S44535 Ferritic Stainless Steel
Cao Xiaoqiang, Jia Jianwen , Yue Xiwen, Hu Qunkun , Wei Yinghui , Hou Lifeng
特殊钢
.
2024, (2): 66
-73
.
DOI: 10.20057/j.1003-8620.2023-00094