热处理工艺及Nb微合金化对9Ni钢组织性能的影响
刘朝霞, 孙宪进, 刘 俊, 叶建军, 王 柯, 徐光琴
Effect of Heat-treatment Process and Nb Microalloying on Microstructure and Properties of 9Ni Steel
Liu Zhaoxia, Sun Xianjin, Liu Jun, Ye Jianjun, Wang Ke, Xu Guangqin
特殊钢
.
2024, (3): 70
-74
.
DOI: 10.20057/j.1003-8620.2023-00172