Mn含量对Inconel718板材焊接接头组织性能的影响
杨亚倩, 马 帅, 王惠生, 杨晓东, 梁 田, 马颖澈
Effect of Mn Content on Microstructure and Properties of Inconel718 Plate Welded Joint
Yang Yaqian, Ma Shuai , Wang Huisheng, Yang Xiaodong, Liang Tian , Ma Yingche
特殊钢
.
2024, (3): 96
-104
.
DOI: 10.20057/j.1003-8620.2023-00176