时效轧制温度对低温取向硅钢组织、织构及磁性能的影响
刘慧丹, 尹利成, 朱继乔, 刘 静, 程朝阳, 戴惠磊
Effect of Aging Rolling Temperature on the Microstructure, Texture and Magnetic Properties of Low-temperature Grain-oriented Silicon Steel
Liu Huidan, Yin Licheng, Zhu Jiqiao, Liu Jing, Cheng Zhaoyang, Dai Huilei
特殊钢
.
2024, (3): 80
-84
.
DOI: 10.20057/j.1003-8620.2023-00181