氮含量与终轧温度对钛微合金化高强钢 CGLC700低温冲击韧性的影响
陈玉凤, 张俊粉, 薛启河, 白 君, 杨树峰, 李京社
Effect of Nitrogen Content and Final Rolling Temperature on Low- temperature Impact Toughness of Titanium Microalloyed High- strength Steel CGLC700
Chen Yufeng, Zhang Junfen, Xue Qihe, Bai Jun, Yang Shufeng, Li Jingshe
特殊钢
.
2024, (3): 40
-18
.
DOI: 10.20057/j.1003-8620.2023-00215