渐进式固溶处理对316H不锈钢组织及性能的影响
荆雪, 辛光瀚, 耿鑫, 姜周华
Effect of Progressive Solid Solution Treatment on the Structure and Properties of 316H Stainless Steel
Jing Xue, Xin Guanghan, Geng Xin, Jiang Zhouhua
特殊钢
.
2025, (1): 99
-105
.
DOI: 10.20057/j.1003-8620.2024-00102