2 100 MPa级桥梁缆索用冷拔钢丝微观组织演变及强化机制
杨旭, 鲍思前, 康筱龙, 胡家瑞, 刘晨, 田仁敏
Microstructure Evolution and Strengthening Mechanism of 2 100 MPa Grade Cold-Drawn Steel Wires for Bridge Cables
Yang Xu, Bao Siqian, Kang Xiaolong, Hu Jiarui, Liu Chen, Tian Renming
特殊钢
.
2025, (1): 92
-98
.
DOI: 10.20057/j.1003-8620.2024-00168