热成型及热处理对小型压力储罐用9Ni钢板力学性能的影响
张军, 沈燕, 于雄
The Influence of Hot Forming and Heat Treatment on the Mechanical Properties of 9Ni Steel Plate for Small Pressure Storage Tanks
Zhang Jun, Shen Yan, Yu Xiong
特殊钢
.
2025, (2): 88
-92
.
DOI: 10.20057/j.1003-8620.2024-00167