690合金显微组织演变对其导热性能的影响
丰涵, 朱永昌, 宋志刚, 顾洋, 刘哲, 杨德博
Effect of Microstructure Evolution on Thermal Conductivity of Alloy 690
Feng Han, Zhu Yongchang, Song Zhigang, Gu Yang, Liu Zhe, Yang Debo
特殊钢
.
2025, (2): 109
-115
.
DOI: 10.20057/j.1003-8620.2024-00200