SUS410半马氏体不锈钢厚壁无缝管内表面裂纹缺陷分析及工艺改进
唐科, 彭俊, 付克刚, 朱萍, 向鑫, 廖凯
Internal Surface Crack Defect Analysis and Process Improvement of SUS410 Semi-Martensite Stainless Steel Thick Wall Seamless Tube
Tang Ke, Peng Jun , Fu Kegang , Zhu Ping, Xiang Xin , Liao Kai
特殊钢
.
2021, (5): 46
-48
.