控轧控冷和冷床保温工艺对42CrMo钢φ50 mm轧材力学性能的影响
金启邦, 孙世平, 王青海, 年国恩, 鲜奋强
Effect of Controlled Rolling and Controlled Cooling and Cooling Bed Heat Preservation Process on Mechanical Properties of 42CrMo Steel φ50 mm Rolled Bar
Jin Qibang, Sun Shiping , Wang Qinghai, Nian Guoen and Xian Fenqiang
特殊钢
.
2021, (5): 72
-74
.