再结晶区轧制工艺参数对X80管线钢组织及织构的影响
叶晓瑜, 黄贞益, 李拔, 陈述, 贾书君, 左军
Affect of Technological Parameter of Recrystallization Zone Rolling on Microstructure and Texture of X80 Pipeline Steel
Ye Xiaoyu, Huang Zhenyi, Li Ba, Chen Shu , Jia Shujun and Zuo Jun
特殊钢
.
2021, (4): 12
-16
.