轻压下和拉速对42CrMo钢410 mm x 530 mm铸坯轧成Φ195 mm材的低倍和中心C偏析的影响
张越, 吕泽安, 马建祎, 钟骞, 王占忠, 彭峰
Effect of Soft Reduction and Cast Speed on Macrostructure and Centre C Segregation of 42CrMo Steel Φ195 mm Bar Rolled from 410 mm x 530 mm Cast Bloom
Zhang Yue, Lii Zean, Ma Jianyi, Zhong Qian, Wang Zhanzhong, Peng Feng
特殊钢
.
2021, (4): 35
-38
.