Computer Simulation on Temperature Field and Phase Transformation of Quenching Heavy Rail End
Zhang Min1 , Zhao Gang1 , Hu Ruihai1 , Li Wenkai1 , Chen Xianzhou2 , Chu Shuangxue2, Dong Maosong2
1. College of Materials Science and Metallurgical Engineering, Wuhan University of Science and Technology, Wuhan 430081 ;
2. Wuhan Iron and Steel Group Corp, Wuhan 430080
Zhang Min , Zhao Gang , Hu Ruihai , Li Wenkai , Chen Xianzhou , Chu Shuangxue, Dong Maosong. Computer Simulation on Temperature Field and Phase Transformation of Quenching Heavy Rail End[J]. Special Steel, 2010, 31(5): 14-17.
[1] 孔祥谦.有限单元法在传热学中的应用.北京:科学出版社,1998
[2] 李辉平,赵国群,栾贻国,等.淬火过程有限元模拟技术的研究现状及其关键技术.山东大学学报,2004,34(5):116
[3] Pan J S,Li Y J,Gu J F. Research and Application Prospect of Computer Simulation on Heat Treatment Process. Journal of Shanghai Jiaotong University ,2000, E-5 (1) :1
[4] 刘 庄,吴肇基,吴景之,等.热处理过程的数值模拟.北京:科学出版社,1996
[5] 程赫明,王洪纲,陈铁力.45钢淬火过程中热传导方程逆向问题求解.金属学报,1997,33(5):467
[6] 杨世铭,陶文铃.传热学.北京:高等教育出版社,1998
[7] Quintana D L,Amitay M,Ortega A,et al. Heat Transfer in the Forced Laminar Wall Jet. Journal of Heat Transfer, 1997,119(3) :451
[8] Cheng He-ming, He Tian-chun, Xie Jian-bin. Solution of an Inverse Problem of Heat Conduction of 45 Steel with Martensite Phase Transformation in High Pressure during Gas Quenching. Journal o£ Materials Science and Technology,2002,18(4) :372