ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2010, Vol. 31 ›› Issue (1): 66-68.

Previous Articles    

Influence of N on Thermoplasticity of Austenite Stainless  Steel 0Crl8Ni9N

Wang Changjun1,2, Zheng Wenjie2, Song Zhigang2, Jiang Yehua1 , Ji Xiangmin2, Feng Han2   

  1. 1 Faculty of Mechanical and Electrical Engineering, Kunming University of Science and Technology, Kunming 650093 ;
    2 Institute for Structural Materials, Central Iron and Steel Research Institute, Beijingl00081)
  • Received:2009-08-19 Online:2010-02-01 Published:2022-10-27

N对奥氏体不锈钢0Crl8Ni9N热塑性的影响

王长军1,2, 郑文杰2, 宋志刚2, 蒋业华1, 季祥民2, 丰涵2   

  1. 1 昆明理工大学机电工程学院,昆明650093;
    2 钢铁研究总院结构材料研究所,北京100081
  • 作者简介:王长军(1984-),男,硕士研究生,控氮奥氏体不锈钢力学性 能和耐蚀性研究。

Abstract: The effect of 0. 008 7% 〜0. 150 0% N on tensile and compression properties of hot-rolled steel 0Crl8Ni9N (% : 0.044 〜0.049C, 0.41 〜0.51Si, 1.46 ~ 1.52Mn, 17. 92 ~ 18. 15Cr, 9.09 〜9.24Ni, 0.01 〜0.03Ti) with strain rate 5 x 10-3s-1 and 1 s-1 at 800 〜130 0 °C has been studied by using Gleeble 1500 thermal simulation machine and the effect of N content on dynamic recrystallization of the steel is analyzed. Results show that with increasing N content in steel the reduction of area of the steel obviously decreases while its optimum temperature range of thermoplasticity increases ; as the N content in steel is less than 0. 050 0% , the optimum temperature range of thermoplasticity of the steel is 950 - 110 0  °C, and as N content is 0.080 0% 〜0. 150 0% , that is 1150 - 1250 °C .

摘要: 采用Gleeble 1500热模拟试验机研究了0.008 7%~0.150 0%N对热轧0Cr18Ni9N钢(%:0.044~0.049C、0.41~0.51Si、1.46~1.52Mn、17.92~18.15Cr、9.09~9.24Ni、0.01~0.03Ti)以应变速率5×10-3s-1和1s-1在800~1300℃的拉伸和压缩性能的影响,并分析了N含量对该钢动态再结晶性能的影响。结果表明,随着N含量的增加,该钢断面收缩率显著下降,同时其最佳热塑性的温度区间提高;当N含量低于0.0500%时,最佳热塑性区间为950~1100℃;而当N含量为0.0800%~0.1500%时,则为1150~1250℃。