Bubble Analysis of Macrostructure of WB36 Thick Wall Seamless Steel Pipe and Process Research
更新时间:2026-01-21
    • Bubble Analysis of Macrostructure of WB36 Thick Wall Seamless Steel Pipe and Process Research

    • Special Steel   Vol. 44, Issue 2, Pages: 29-32(2023)
    • DOI:10.20057/j.1003-8620.2022-00127    

      CLC:
    • Received:08 October 2022,

      Online First:27 March 2023,

      Published:27 March 2023

    移动端阅览

  • 夏云峰, 周仲成, 胡永平, et al. Bubble Analysis of Macrostructure of WB36 Thick Wall Seamless Steel Pipe and Process Research[J]. Special Steel, 2023, 44(2): 29-32. DOI: 10.20057/j.1003-8620.2022-00127.

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Development of Continuous Casting Round Billet for P92 Heat-resistant Steel for Ultra-supercritical Boiler Tubes
Numerical Simulation and Process Practice of Mold Electromagnetic Stirring for IF Steel Slab

Related Author

Gong Zhixiang
Wang Kaizhong
Hu Fangzhong
Chen Enxin
Yang Zhiqiang
Liu Qilong
Deng Yong
Li Huagang

Related Institution

Special Steel Company of Ma'anshan Iron and Steel Co., Ltd.
No.4 Steelmaking and Rolling General Plant of Ma’anshan Iron & Steel Co.,Ltd., Ma’anshan
Intelligent Equipment Business Division of Shanghai BAOSIGHT Soft Co.,Ltd.
0