Systems Engineering Considerations for the Electric Arc Furnace Steelmaking Process
Smelting and Solidification | 更新时间:2026-01-21
    • Systems Engineering Considerations for the Electric Arc Furnace Steelmaking Process

    • Special Steel   Vol. 44, Issue 4, Pages: 74-79(2023)
    • DOI:10.20057/j.1003-8620.2023-00041    

      CLC: TF087
    • Received:16 March 2023,

      Published:01 August 2023

    移动端阅览

  • Chen Yu,Zhao Ruimin,Wei Guangsheng.Systems Engineering Considerations for the Electric Arc Furnace Steelmaking Process[J].Special Steel,2023,44(04):74-79. DOI: 10.20057/j.1003-8620.2023-00041.

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Investigation and Analysis of the Production Efficiency of Electric Furnace Steelmaking

Related Author

Miao Liang

Related Institution

Development Department, CITIC Pacific Special Steel Group Co., Ltd., Jiangyin
0