您当前的位置:
首页 >
文章列表页 >
Continuous Cooling Phase Transformation Prediction Model of 20CrMnTiH
Forming and Phase Transition | 更新时间:2025-05-09
    • Continuous Cooling Phase Transformation Prediction Model of 20CrMnTiH

    • Special Steel   Vol. 45, Issue 1, Pages: 82-86(2024)
    • DOI:10.20057/j.1003-8620.2023-00114    

      CLC: TG142
    • Received:10 June 2023,

      Published:30 January 2024

    移动端阅览

  • Yang Ting,Duan Luzhao,Liu Xu,et al.Continuous Cooling Phase Transformation Prediction Model of 20CrMnTiH[J].Special Steel,2024,45(01):82-86. DOI: 10.20057/j.1003-8620.2023-00114.

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Research and Development of 10B38 Boron Containing Cold Heading Steel
Effect of Holding Technology at Intermediate Roll Table in Hot Continuous Rolling on Phase Transformation and Structure of Low Carbon Steel
Finite Element Analysis on Temperature Field of Finishing Rolled 20CrMnTiH Steel Round Bar during Controlled Cooling
Effect of Cooling Rate of Hot-Deformed Austenite on Structure and Property of X80 Pipeline Steel
Continuous Cooling Transformation Curves of Steel 30CrMo Produced by Thin Slab Casting and Rolling Process and Its Application

Related Author

Guo Dayong
Ma Liguo
Pan Yang
Zhang Bo
Gao Hang
Wang Bingxi
徐远军
赵刚

Related Institution

Ansteel Group Iron and Steel Research Institue
State Key Laboratory of Metal Material for Marine Equipment and Application
武汉科技大学材料与冶金学院
武汉钢铁公司
北京科技大学材料科学与工程学院
0