Effect of La Treatment on Inclusions in H13 Hot Work Die Steel
Smelting and Solidification | 更新时间:2025-05-09
    • Effect of La Treatment on Inclusions in H13 Hot Work Die Steel

    • Special Steel   Vol. 45, Issue 4, Pages: 117-123(2024)
    • DOI:10.20057/j.1003-8620.2024-00092    

      CLC: TG142
    • Received:15 April 2024,

      Published:30 July 2024

    移动端阅览

  • Ren Ji,Yan Yun,Tian Jialong,et al.Effect of La Treatment on Inclusions in H13 Hot Work Die Steel[J].Special Steel,2024,45(04):117-123. DOI: 10.20057/j.1003-8620.2024-00092.

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

2

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Effect of Different Residual Steel Amounts on Molten Steel Cleanliness
Development of Continuous Casting Round Billet for P92 Heat-resistant Steel for Ultra-supercritical Boiler Tubes
Research on the Metallurgical Properties of Fluorine-Containing Refining Slag and Its Fluoride-Free Design
Optimization of Electromagnetic Parameters for the 3rd-generation FC MOLD
Effect of Rare Earth Ce on the Evolution of Inclusions in 20MnTiB Cold Heading Steel

Related Author

Ren Ying
Liu Zhonghua
Wang Bochen
Lu Boxun
Zhang Hejun
Zhang Lifeng
Gong Zhixiang
Wang Kaizhong

Related Institution

School of Mechanical and Materials Engineering, North China University of Technology
Tangshan Iron and Steel Group Co., Ltd., Steelmaking Division
School of Metallurgical and Ecological Engineering,University of Science and Technology Beijing
Metallurgical Corporation of China (MCC) CADI Ironmaking Division
Tangshan Iron and Steel Group Co., Ltd., Research and Development Center
0