The Metallurgical Mechanisms of Inclusions in the FGH4096 Alloy during Electron Beam Refining
Smelting and Solidification | 更新时间:2025-05-09
    • The Metallurgical Mechanisms of Inclusions in the FGH4096 Alloy during Electron Beam Refining

    • Special Steel   Vol. 45, Issue 4, Pages: 47-54(2024)
    • DOI:10.20057/j.1003-8620.2024-00117    

      CLC: TF806.81;TG132.3
    • Received:29 April 2024,

      Published:30 July 2024

    移动端阅览

  • Dong Liyang,You Xiaogang,Dong Gengyi,et al.The Metallurgical Mechanisms of Inclusions in the FGH4096 Alloy during Electron Beam Refining[J].Special Steel,2024,45(04):47-54. DOI: 10.20057/j.1003-8620.2024-00117.

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

0

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Effect on Fatigue Failure Behavior Induced by Inclusions in GCr15 Bearing Steel Under Different Metallurgical Processes
High Temperature Mechanical Properties and Fracture Mechanism of 9Cr-2W-3Co Martensitic Heat-resistant Steel
Effect of LF Soft Bubbling Time on Inclusions in Tire Cord Steel LX82 A
Numerical Simulation and Industrial Experiment of Vacuum Arc Remelting ϕ690 mm Large-sized GH4738 Superalloy Ingot
Effect of Magnetic-Controlled Electroslag Remelting on Solidification Microstructure and Mechanical Properties of M2 High-speed Steel

Related Author

Wang Zheng
Chen feng
Shi Tao
Yin Qing
Hu Bin
Luo Haiwen
Geng Wei
Zhu Zhibao

Related Institution

Jiangying Xingcheng Special Steel Works Co., Ltd., Jiangying
School of Metallurgy and Ecological Engineering, University of Science and Technology Beijing
Changzhou Baoling Heavy & Industrial Machinery Co., Ltd.
Daye Special Steel Co., Ltd.
State Key Laboratory of Advanced Refractories, Wuhan University of Science andTechnology
0