您当前的位置:
首页 >
文章列表页 >
Analysis of Fracture Split Defects of Non-Quenched-Tempered Steel 36MnVS4 Connecting Rods and Controlled Forging and Cooling Process Tests
Forming and Phase Transition | 更新时间:2026-07-14
    • Analysis of Fracture Split Defects of Non-Quenched-Tempered Steel 36MnVS4 Connecting Rods and Controlled Forging and Cooling Process Tests

    • Special Steel   Vol. 47, Issue 4, Pages: 103-108(2026)
    • DOI:10.20057/j.1003-8620.N250565    

      CLC: TG306
    • Received:18 October 2025,

      Revised:2026-01-13,

      Accepted:16 January 2026,

      Published:30 July 2026

    移动端阅览

  • Xian Fenqiang,Wang Leiying,Jiang Bo,et al.Analysis of Fracture Split Defects of Non-Quenched-Tempered Steel 36MnVS4 Connecting Rods and Controlled Forging and Cooling Process Tests[J].Special Steel,2026,47(04):103-108. DOI: 10.20057/j.1003-8620.N250565.

  •  
  •  
icon
试读结束,您可以激活您的VIP账号继续阅读。
去激活 >
icon
试读结束,您可以通过登录账户,到个人中心,购买VIP会员阅读全文。
已是VIP会员?
去登录 >

0

Views

63

下载量

0

CSCD

0

CNKI被引量

>
Alert me when the article has been cited
提交
Tools
Download
Export Citation
Share
Add to favorites
Add to my album

Related Articles

Effect of Ca-Si Treatment on Morphology and Ingredient of Sulfide in Free Cutting Non-Quenching-Tempering Steel 30MnVS
A Study on Recrystallization of Non-Quenched-Tempered Steel 40Mn2V during Thermal Deformation
R & D Present Status and Progress of High Strength Ship Plate Steel At Home and Abroad
Effect of Forging Methods on the Isotropy of FS450 Modules
Numerical Simulation of the Effect of Pouring Process on Solidification Cracking in P92 Steel Ingots

Related Author

袁婷
李国忠
周兴海
涂益友
蒋建清
邹喜洋
谢凯意
袁泽喜

Related Institution

东南大学江苏省先进金属材料高技术研究重点实验室
兴澄特种钢铁有限公司,江阴
武汉科技大学钢铁冶金及资源利用省部共建教育部重点实验室
湖南衡阳华菱钢管(集团)有限公司技术中心
鞍钢股份公司技术中心
0