最新刊期

    卷 47 , 期 6 , 2026
    整期导读

      Product Research and Development

    • Huang Yongzhi, Gao Zhiming, Lü Chuantao, Chen Pengfei
      Vol. 47, Issue 6, Pages: 1-6(2026) DOI: 10.20057/j.1003-8620.N260037
      摘要:Aiming at the bottleneck of severe corrosion failure of conventional casing and tubing in the development of deep, ultra-deep and high-sour oil and gas fields in China, a systematic study on key technologies of high-performance bimetallic metallurgically bonded composite OCTG was carried out. By adopting an innovative material system of "high-strength sour-service low alloy steel outer layer + corrosion-resistant alloy (CRA) inner layer", the critical chemical composition ranges (mass fraction) of the outer sour-service low alloy steel ( ≤ 0.008%P, ≤ 0.002%S, 0.50%-1.00%Cr, 0.20%-0.40%Mo) and the main composition of the inner 20-40 type nickel-based CRA (20.00%-23.00% Cr, ≥40.00% Ni, 5.00%-8.00% Mo) were determined. A short-process manufacturing route combining "electroslag remelting (ESR) composite billet + controlled rolling and cooling" was developed, through which the key process parameters were established: ESR melting rate controlled at 5.0-6.5 kg/min, initial hot rolling temperature of 1 150-1 200 ℃, finish rolling temperature ≥ 900 ℃, cumulative reduction ≥ 60%, quenching temperature of 900-950 ℃, and tempering temperature of 600-680 ℃. For the ϕ88.9 mm×7.34 mm composite pipe, the interfacial shear strength reached 572-585 MPa, and the tensile strength of the outer low alloy steel was 865-982 MPa. Under simulated harsh service conditions, the uniform corrosion rate was ≤ 0.003 mm/a, which was two orders of magnitude lower than the industry standard. This achievement has been demonstrated in engineering applications in highly corrosive oil and gas fields, providing technical support for the safe and efficient development of deep oil and gas resources in China.  
      关键词:Bimetallic Composite Pipes;Oil Tubing and Casing;Corrosion-Resistant Materials;Short-Process Manufacturing;Premium Threaded Connections   
      19
      |
      14
      |
      0
      <HTML>
      <L-PDF><WORD><Meta-XML>
      <引用本文> <批量引用> 159005559 false
      更新时间:2026-11-16
    • Yuan Changbo, Zhu Lei, Wang Yufeng, Dou Shengtao, Li Guoqiang, Shi Quanqiang, Wang Wei
      Vol. 47, Issue 6, Pages: 7-12(2026) DOI: 10.20057/j.1003-8620.N250602
      摘要:Based on currently commercial non-quenched and tempered steels, this study innovatively proposes a compositional design strategy of “reduced C, increased Si, and added Mn”. Through compositional regulation and microstructural optimization, a novel high-strength, high-toughness, and low-cost non-quenched and tempered steel with a tensile strength of approximately 1 300 MPa was successfully developed. The results indicate that the novel non-quenched and tempered steel (QGF17) has the following chemical composition (w/%): 0.19C, 1.92Si, 2.90Mn, 0.56Cr, 0.012P, and 0.004S. The addition of Si optimizes the bainitic microstructure, leading to an increased volume fraction of lath bainite (LB). Meanwhile, the grain size is refined from 18 μm to 11 μm, the fraction of high-angle grain boundaries (HAGBs) increases markedly from 28.5% to 59.1%, and the dislocation density also rises. As a result, localized high-dislocation-density regions form near grain boundaries and lath interfaces. Compared with FAS2225 steel, the novel non-quenched and tempered steel exhibits substantially improved, especially the hardness and mechanical properties. The HV hardness increases from 318 to 473, the yield strength and tensile strength rise from 710 MPa and 955 MPa to 973 MPa and 1 322 MPa, respectively, and the impact energy at -20 °C increases significantly from 16 J to 29 J. In addition, the novel steel demonstrates a higher strain-hardening capability and excellent impact toughness. The SEM fracture analysis reveals that although both steels exhibit quasi-cleavage fracture characteristics under impact loading, a pronounced plastic deformation zone is observed near the V-notch region in the novel non-quenched and tempered steel. Correspondingly, the fracture morphology evolves from river-pattern quasi-cleavage facets in FAS2225 steel to finer quasi-cleavage micro-facets in the novel steel. These results confirm that, through simplified alloying and optimized compositional design, the developed non-quenched and tempered steel effectively reduces production costs while overcoming the long-standing trade-off between strength enhancement and toughness degradation in conventional high-strength non-quenched steels, thereby providing a promising technological pathway for the engineering application of high-performance non-quenched and tempered steels.  
      关键词:Non-quenched and Tempered Steel;Silicon;Low-temperature Impact Toughness;High-Angle Grain Boundary(HAGB);Quasi-cleavage Fracture   
      180
      |
      366
      |
      0
      <HTML>
      <L-PDF><WORD><Meta-XML>
      <引用本文> <批量引用> 149536486 false
      更新时间:2026-11-16

      Smelting and Solidification

    • Leng Zihan, Jiang He, Zhu Xiongming, Dong Jianxin
      Vol. 47, Issue 6, Pages: 13-23(2026) DOI: 10.20057/j.1003-8620.N260068
      摘要:GH3625 is a typical high-temperature alloy, and its smelting process is usually carried out using a duplex process. However, some processes are invisible, making parameter measurement and result prediction challenging. In such cases, numerical simulation methods are required to investigate the relevant processes. For the VIM and ESR process control of GH3625 alloy, by combining Procast and Meltflow software and constructing a computational model, the solidification process can be simulated and analyzed, and the influence of tooling dimensions and process parameters on the VIM and ESR processes can be revealed. The results show that for ϕ400 mm ingots of GH3625 alloy, without using risers in vacuum induction melting and casting, a shrinkage cavity as deep as 580 mm forms at the head of the ingot. Increasing the riser height can significantly reduce defects; reducing the pouring speed can shorten the length of the internal shrinkage cavity, amd the length at a pouring speed of 7 kg/s is 300 mm shorter than that at 13 kg/s. Increasing the mold preheating temperature increases the volume of the internal shrinkage porosity and cavity. During the electroslag remelting process, as the slag height increases, the peak value of secondary dendrite spacing increases by 20 μm, and the probability of spot segregation decreases; as the remelting rate increases, the width of the mushy zone increases from 160 mm to 200 mm. This method and related research results provide theoretical references for process optimization in the VIM and ESR smelting processes of GH3625 alloy.  
      关键词:Superalloy GH3625;Vacuum Induction Melting;Electroslag Remelting;Porosity and Shrinkage Cavity;Solidification   
      22
      |
      12
      |
      0
      <HTML>
      <L-PDF><WORD><Meta-XML>
      <引用本文> <批量引用> 160045721 false
      更新时间:2026-11-16
    • Tang Chao, Huang Yufei, Qiao Xiya, Yang Xin, He Zhijun
      Vol. 47, Issue 6, Pages: 24-33(2026) DOI: 10.20057/j.1003-8620.N260010
      摘要:The service performance of GCr15SiMn bearing steel, a core material for critical components in high-end manufacturing, is highly sensitive to the mechanical properties of non-metallic inclusions. This study investigates CaO-SiO2-Al2O3 composite inclusions in GCr15SiMn steel and systematically examines the effect of the w(CaO)/w(SiO2) on their phase composition, silicate network structure, and micromechanical properties using X-ray diffraction, Raman spectroscopy, and nanoindentation. The results show that the inclusions initially form as amorphous glassy phases, and their crystallinity increases significantly with increasing w(CaO)/w(SiO2). The phase composition evolves from an amorphous-dominated structure at low w(CaO)/w(SiO2) to stable crystalline phases such as CaSiO3, CaAl2Si2O8, and CaAl2O4 at high w(CaO)/w(SiO2). With increasing w(CaO)/w(SiO2), the silicate network undergoes pronounced depolymerization: the fraction of medium and high-polymerization units decreases, while that of low-polymerization units increases, accompanied by a continuous rise in non-bridging oxygen content. In terms of mechanical properties, the hardness of the inclusions generally decreases, whereas the elastic modulus increases steadily to 104.04 GPa. The fracture resistance parameter H3/E2 decreases from 0.071 GPa to 0.052 GPa, and the energy dissipation ratio Wp/Weincreases from 0.99 to 1.2. Inclusions with low w(CaO)/w(SiO2) possess a highly polymerized and dense network structure, endowing them with superior hardness and damage resistance, which contributes to enhanced overall hardness and damage tolerance of the GCr15SiMn bearing steel.  
      关键词:GCr15SiMn Bearing Steel;Inclusions;Amorphous Phase;Silicate Network;Mechanical Property   
      121
      |
      45
      |
      0
      <HTML>
      <L-PDF><WORD><Meta-XML>
      <引用本文> <批量引用> 156317024 false
      更新时间:2026-11-16
    • Zhang Zhixiao, Chou Hongye, Jin Congjin, Gao Ruiquan, Yu Yong, Qu Tianpeng, Wang Deyong
      Vol. 47, Issue 6, Pages: 34-39(2026) DOI: 10.20057/j.1003-8620.N260062
      摘要:Taking a 100 t ladle from a steel plant as the research object, a combination of physical simulation and numerical simulation was employed to systematically study the effects of bottom argon blowing parameters on fluid flow, mixing time, slag eye formation, and wall shear stress inside the ladle. By comparing different types of permeable plugs, bottom blowing flow rates, and positions, the evolution law of the flow field and the utilization mechanism of stirring energy were revealed. The results show that the stirring effect of diffusive plugs is superior to that of slotted plugs, and increasing the bottom blowing flow rate significantly reduces the mixing time. The optimal eccentricity for single-plug bottom blowing is 0.75R, and either excessively low or high eccentricity is detrimental to the effective utilization of stirring energy. The mixing effect of dual-plug bottom blowing is significantly influenced by the angle between the plugs. At an eccentricity of 0.6R and an angle of 135°, the minimum mixing time is obtained, and this configuration effectively reduces the slag eye area and wall shear stress, thereby mitigating refractory erosion.  
      关键词:Bottom Argon Blowing;Physical Simulation;Numerical Simulation;Mixing Time;Slag Eye Formation;Wall Shear Stress   
      30
      |
      13
      |
      0
      <HTML>
      <L-PDF><WORD><Meta-XML>
      <引用本文> <批量引用> 160044697 false
      更新时间:2026-11-16
    • Miao Zhiqi, Yin Qing, Lu Changhe, Hua Liukai, Guan Yuehui, Cheng Guoguang
      Vol. 47, Issue 6, Pages: 40-46(2026) DOI: 10.20057/j.1003-8620.2025-00153
      摘要:The evolution mechanism of CaO content in inclusions during VD treatment was studied through industrial experiments and thermodynamic calculations, and the effects of steel liquid and slag composition on steel slag reaction were analyzed. The study found that after the VD process, the CaO content in the slag decreased by 14%, while the Al content in the molten steel had a burning loss rate of up to 70%, indicating that a intense steel slag reaction occurred during the VD process. The average CaO mass fraction in the inclusions increased from 6.8% before VD to 11.3%, and the inclusion size increased. The ideal dynamic conditions and the evaporation of Ca during the VD process jointly trigger and were expected to further enhance the chemical reaction between Al in the molten steel and CaO in the slag, allowing Ca in the slag to enter the molten steel. Some of the dissolved Ca will come into contact with low CaO or CaO free inclusions in the molten steel and react, resulting in an increase in CaO content in the inclusions.In order to suppress the steel slag reaction during the VD process, measures such as increasing the Al2O3 content in the slag and increasing the pressure during the VD process can be taken.  
      关键词:Bearing Steel;VD;Inclusions;Steel Slag Balance   
      73
      |
      198
      |
      0
      <HTML>
      <L-PDF><WORD><Meta-XML>
      <引用本文> <批量引用> 126430756 false
      更新时间:2026-11-16
    • Jia Yuting, Wang Zhiyuan, Li Shisen, Jing Yuan, Kong Lingzhong, Yang Jie, Zang Ximin
      Vol. 47, Issue 6, Pages: 47-53(2026) DOI: 10.20057/j.1003-8620.N260082
      摘要:To address the engineering issue of surface cracking in the production of large-sized P92 steel ingots, this study established a thermo-mechanical coupling model for 19 t P92 martensitic heat-resistant steel ingot casting with a height of 2 720 mm using ProCAST simulation software. The thermophysical property parameters of P92 steel were obtained by JMatPro calculations and on-site production measurements. On this basis, the effects of pouring temperature and pouring rate on the stress field of the 19 t P92 steel ingot were systematically investigated. Numerical simulation results indicate that the bottom of the ingot tail is a zone prone to severe stress concentration, and the pits at the edge of the ingot tail serve as the critical risk zones for hot cracking initiation. At pouring temperatures of 1 540, 1 550 and 1 560 ℃, the stress concentration intensifies with increasing pouring temperature, and maximum stress values all appear at the pits on the ingot tail edge. Compared with the high-temperature pouring condition at 1 560 ℃, low-temperature pouring at 1 540 ℃ reduces the maximum stress at this position by 4.7%. When the pouring rates are set as 2, 3 and 4 t/min respectively, increasing the pouring rate intensifies the cracking tendency. The maximum principal stress at the edge at a low pouring rate (2 t/min) is 9% lower than that at a high pouring rate (4 t/min). To mitigate the hot cracking risk at the ingot tail, a low pouring rate process with a temperature of (1 550 ± 5) ℃ is recommended. This process can effectively relieve stress concentration and reduce the hot cracking risk.  
      关键词:Large Steel Ingot;P92 Martensitic Heat-resistant Steel;Cracking;Stress Field   
      21
      |
      13
      |
      0
      <HTML>
      <L-PDF><WORD><Meta-XML>
      <引用本文> <批量引用> 161211938 false
      更新时间:2026-11-16
    • Wang Yan, Gu Yu, Li Jidong, Fan Xinzhi
      Vol. 47, Issue 6, Pages: 54-59(2026) DOI: 10.20057/j.1003-8620.N260054
      摘要:N06625 nickel-based alloy plates were produced by two different process routes, namely VIM+ESR and EAF+AOD+continuous casting. The segregation characteristics, microstructure and mechanical properties were systematically investigated by means of mechanical testing machine, optical microscope, SEM, EDS and electron probe microanalyzer. The results show that the segregation degrees of Mo and Nb in the continuous casting slab are lower than those in the conventional electroslag ingot, providing favorable conditions for subsequent homogenization treatment and hot working. Owing to the finer original dendrites and milder segregation, the continuous casting slab requires a shorter homogenization holding time to eliminate elemental segregation and exhibits better process applicability. Under the actual production conditions in this work, the optimal homogenization parameters for the ϕ600 mm electroslag ingot are 1 240 ℃ for 48 h, while the parameters for the 180 mm-thick continuous casting slab are 1 240 ℃ for 36 h. The mechanical properties, inclusion characteristics and corrosion resistance of the plates manufactured by the two process routes are at the same technical level. The corrosion rates of the VIM+ESR route measured by ASTM G28A, ASTM A262C and ASTM G48A are 0.024 mm/month, 0.03 mm/month and 0 g/m2, respectively; the corresponding values of the EAF+AOD+continuous casting route are 0.021 mm/month, 0.03 mm/month and 0 g/m2.  
      关键词:N06625 Nickel-Based Alloy;Plate;Continuous Casting;Segregation;Homogenization   
      163
      |
      58
      |
      0
      <HTML>
      <L-PDF><WORD><Meta-XML>
      <引用本文> <批量引用> 157871297 false
      更新时间:2026-11-16

      Forming and Phase Transition

    • Effect of Forging Methods on the Isotropy of FS450 Modules

      Ouyang Weihao, Feng Liang, Hai Yongxiu, Ma Ye, Lin Jingjing, Wang Jian, Bi Yuhan
      Vol. 47, Issue 6, Pages: 60-64(2026) DOI: 10.20057/j.1003-8620.N260097
      摘要:The effect of the forging process on the isotropy and impact properties of hot work die steel FS450 (4Cr5Mo2V), smelted by EAF + LF + VD + protective atmosphere electroslag remelting, was investigated using optical microscopy, scanning electron microscopy, and impact testing. A comparative analysis was conducted on the microstructure and properties of the steel processed by two methods: the axial repeated upsetting and drawing method and the multi-directional forging (MDF) method. The spheroidized microstructures of the tested steels produced by both processes reached AS4 level according to NADCA#207 standard. However, MDF significantly alleviated the banded segregation. In terms of impact properties, the average transverse and longitudinal impact absorbed energies of the MDF specimens were 25.1 J and 26.2 J, respectively, with a transverse-to-longitudinal ratio of 0.96. For the axial repeated upsetting and drawing specimens, the corresponding values were 20.6 J and 24.8 J, with a ratio of 0.83. The impact fracture surfaces of the MDF specimens exhibited larger and deeper dimples, fewer quasi-cleavage planes, and more numerous tearing ridges, indicating better toughness. After quenching and tempering, the microstructures of both tested steels consisted of tempered martensite with dispersed carbides, and the grain sizes were both finer than Grade 7. Nevertheless, the MDF process resulted in a more uniform and finer grain structure. In summary, the MDF method improves microstructural uniformity and alleviates banded segregation, thereby significantly enhancing the impact toughness and isotropy of FS450 steel, outperforming the conventional axial repeated upsetting and drawing process.  
      关键词:Die Steel;Forging;Impact Toughness;Isotropy   
      14
      |
      13
      |
      0
      <HTML>
      <L-PDF><WORD><Meta-XML>
      <引用本文> <批量引用> 165357671 false
      更新时间:2026-11-16
    • Zhou Lei, Wang Fei
      Vol. 47, Issue 6, Pages: 65-72(2026) DOI: 10.20057/j.1003-8620.N260030
      摘要:The thermal compression deformation behavior and microstructure evolution of 2 200 MPa ultra-high-strength steel were experimentally investigated using a Thermomastor-Z thermal simulation machine. Stress-strain curves under different strain rates (0.01 s⁻¹, 1 s⁻¹, and 5 s⁻¹) and deformation temperatures (850–1 150 ℃) with an engineering strain of 60% were tested. By analyzing the stress-strain curves and conducting EBSD analysis on deformed samples, the effects of strain rates and temperatures on the deformation resistance and dynamic recrystallization process of 2 200 MPa ultra-high-strength steel were studied. The recrystallization activation energy of the experimental steel was determined through regression calculations. The results indicate, 1) Higher deformation temperatures and lower strain rates result in lower deformation resistance of 2 200 MPa ultra-high-strength steel; 2) Dynamic recrystallization is activated at the strain rate of 0.01 s⁻¹ when the temperature ≥900 ℃; at strain rates of 1 s⁻¹ and 5 s⁻¹, dynamic recrystallization is activated when the temperature ≥1 000 ℃. During hot working processing, higher strain rates should be applied at temperatures ≥1 000 ℃, while lower strain rates are recommended below 1 000 ℃; 3) The calculated recrystallization activation energy of 2200 MPa ultra-high-strength steel is 421.20 kJ/mol; 4) A constitutive model for the flow stress of 2 200 MPa ultra-high-strength steel was established.  
      关键词:2 200 MPa-grade Ultra-High Strength Steel;Thermal Simulation;Hot Deformation Behavior;Dynamic Recrystallization;Recrystallization Activation Energy   
      101
      |
      39
      |
      0
      <HTML>
      <L-PDF><WORD><Meta-XML>
      <引用本文> <批量引用> 156319022 false
      更新时间:2026-11-16
    • Zhou Yang, Yang E, Xie Yumin, Zhang Xiaofeng, Wu Tianhua, Shi Zhongyi, Yu Ketian
      Vol. 47, Issue 6, Pages: 73-77(2026) DOI: 10.20057/j.1003-8620.N250593
      摘要:To study the continuous cooling transformation behavior of 4330V low alloy high strength steel, experiments were conducted at different cooling rates 0.05-30 ℃/s using a quenching dilatometer. Optical microscopy, field emission scanning electron microscopy, and microhardness tester were used to detect and analyze the microstructure and Vickers hardness of the material after phase transformation at different cooling rates, and the continuous cooling transformation (CCT) curve of its supercooled austenite was plotted. The results showed that when the cooling rate was 0.05-0.15 ℃/s, the microstructure was mainly bainite + ferrite, belonging to the high-temperature and medium-temperature two-phase composite transformation zone, and the hardness values were all below 450 HV; when the cooling rate was 0.2-1 ℃/s, the microstructure was mainly bainite + martensite, belonging to the medium-temperature and low-temperature two-phase composite transformation zone, and the hardness was between 472-577HV; when the cooling rate was greater than or equal to 3 ℃/s, the microstructure was fully martensitic, belonging to the low-temperature martensitic transformation zone, and the hardness values were all above 593 HV.  
      关键词:4330V Low Alloy High Strength Steel;Continuous Cooling Transformation;CCT curve;Microstructure;Hardness   
      164
      |
      52
      |
      0
      <HTML>
      <L-PDF><WORD><Meta-XML>
      <引用本文> <批量引用> 149532957 false
      更新时间:2026-11-16
    • Sun Changliang, Xin Guanghan, Geng Xin
      Vol. 47, Issue 6, Pages: 78-86(2026) DOI: 10.20057/j.1003-8620.N250591
      摘要:Hot-work die steel(DHA) steel was selected as the research object and adds Niobium (Nb) elements with mass fractions of 0, 0.009%, 0.019%, 0.028%, and 0.038% to the steel. The influence of Nb on the microstructure and mechanical properties of DHA steel was investigated. The results show that Nb addition promotes the formation of large-sized primary carbonitrides during solidification, and aggravates the secondary dendrites segregation in the as-cast microstructure. Nb addition refines the grain size of the experimental steel after tempering. With the increase of Nb mass fraction, toughness gradually decreases after tempering at 560 ℃ and 590 ℃, and first increases and then decreases after tempering at 620 ℃. Strength first increases and then decreases with increasing Nb content. Considering the comprehensive mechanical properties, when the mass fraction of Nb element is 0.019%, DHA steel has the best performance.  
      关键词:Hot-work Die Steel;Niobium Content;Microstructure;Mechanical Properties   
      156
      |
      166
      |
      0
      <HTML>
      <L-PDF><WORD><Meta-XML>
      <引用本文> <批量引用> 149533021 false
      更新时间:2026-11-16
    • Zhang Yongwei, Liu Zhihao, Zhang Qingxue, Qian Yajun, Chen Minxia, Deng Xiangtao
      Vol. 47, Issue 6, Pages: 87-93(2026) DOI: 10.20057/j.1003-8620.N260047
      摘要:The microstructure, mechanical properties, wear resistance, and wear mechanism of NM550RE steel alloyed with 0.001 2% rare-earth w[Ce] were systematically studied, and compared them with those of conventional NM550 steel. The results show that the conventional NM550 steel has an average original austenite grain size of 9.48 μm and a hardness of 553HBW. The addition of Ce refines the grain size, reducing the average austenite grain size to 7.55 μm and increasing the hardness to 579HBW. Meanwhile, the impact energy at -40 °C increases from 29.43 J to 34.63 J. The G65 abrasive wear test results show that the wear resistance of NM550RE steel is 1.11 times that of conventional NM550 steel. After rare-earth modification, the inclusions exhibit better compatibility with the matrix, while the steel possesses a fine grain size, higher hardness, and toughness. During wear, this helps hinder abrasive particles from penetrating into the matrix and prevents further development of ploughing grooves, thereby reducing their width and depth and resulting in superior wear resistance.  
      关键词:Rare Earth Element Ce;Abrasive Wear;Wear Resistance;Wear Mechanism   
      144
      |
      41
      |
      0
      <HTML>
      <L-PDF><WORD><Meta-XML>
      <引用本文> <批量引用> 155598317 false
      更新时间:2026-11-16
    • Guo Biaobiao, Wang Rui, Zhang Yu, Yan Zhijie, Wang Zhigang, Shi Zhiyue, Kang Yan, Yu Zhiqiang, Li Fenghao
      Vol. 47, Issue 6, Pages: 94-103(2026) DOI: 10.20057/j.1003-8620.N260023
      摘要:Fe-13Cr-0.7C-0.3V martensitic stainless steel is widely used in various fields due to its high strength and hardness. However, its high carbon and high alloy content lead to the precipitation of networked carbides during solidification, which severely deteriorates the mechanical properties of the steel. In this paper, (Differential Scanning Calorimetry)DSC was used to determine the phase transformation temperatures of the hot-rolled Fe-13Cr-0.7C-0.3V martensitic stainless steel. The effect of austenitizing temperature on the microstructure and properties of the test steel was investigated, and the appropriate quenching temperature was determined; on this basis, the influence of tempering temperature in the range of 100-700 ℃ on its microstructure and properties was studied in depth. Experimental evidence validates that the austenite start and finish for the transformation of ferrite to austenite of Fe-13Cr-0.7C-0.3V steel are 834.3 ℃and 879.6 ℃, respectively. In the course of austenitizing temperature elevation, the introduction of V inhibits the dissolution and coarsening of carbides and refines their particle size; meanwhile, the volume fraction of retained austenite increases, resulting in reduced hardness of the material. During tempering, the increase in temperature promotes the decomposition of martensite, and supersaturated carbon precipitates from the solid solution to form dispersed carbides. A tensile strength of 1 930 MPa and fracture elongation of 3.8% are achieved through tempering at 200 ℃.  
      关键词:Martensitic Stainless Steel;Heat Treatment;Carbides;Mechanical Properties;Microstructure   
      146
      |
      53
      |
      0
      <HTML>
      <L-PDF><WORD><Meta-XML>
      <引用本文> <批量引用> 156511320 false
      更新时间:2026-11-16

      Application and Service

    • Wei Zhen, Huo Jie, Yi Pengyue, Li Xiao, Li Hongmei
      Vol. 47, Issue 6, Pages: 104-111(2026) DOI: 10.20057/j.1003-8620.N260043
      摘要:The coarse and non-uniform grain structures arising from microstructural heredity in large rotors fabricated from 9Cr-3 W-3Co martensitic heat-resistant steel present a significant challenge to mechanical property uniformity. This study investigates the influence of isothermal annealing pretreatment (single-step and stepwise) in conjunction with tempering temperature (700 ℃, 710 ℃, and 720 ℃) on microstructural homogeneity and mechanical properties. Both annealing routes, followed by normalizing, refined the prior austenite grains to ASTM No. 7.0 or finer. Notably, stepwise isothermal annealing substantially enhanced the spatial uniformity of the grain size and effectively mitigated the post-forging microstructural heredity. Following quenching and tempering, differences in strength and ductility between specimens subjected to the different isothermal annealing cycles were negligible (<5%). However, stepwise annealing significantly improved impact toughness and reduced data scatter. Tempering temperature was identified as the dominant factor controlling the strength-toughness balance: increasing the tempering temperature from 700 ℃ to 720 ℃, decreased the tensile strength from 852 MPa to 817 MPa, while concurrently increasing the impact absorbed energy from 22.3 J to 33.3 J. The optimal combination of properties (Rm >830 MPa, Rp0.2 >680 MPa, impact energy >24 J) was achieved through stepwise isothermal annealing followed by tempering at 710 ℃. This improvement is primarily attributed to the refinement and homogeneous distribution of carbides, as well as improved prior austenite grain uniformity. These findings provide a critical theoretical and experimental foundation for the engineering application of this material in 630 ℃ ultra-supercritical high-pressure turbine rotors.  
      关键词:Martensitic Heat-resistant Steel;Stepwise Isothermal Annealing;Tempering Temperature;Grain Refinement;Strength-toughness Balance   
      129
      |
      56
      |
      0
      <HTML>
      <L-PDF><WORD><Meta-XML>
      <引用本文> <批量引用> 155797465 false
      更新时间:2026-11-16
    • Yang Yang, Yuan Qing, Li Zhongbo, Xu Shaopu, Li Liang, Tang Zhenglei
      Vol. 47, Issue 6, Pages: 112-119(2026) DOI: 10.20057/j.1003-8620.N260055
      摘要:The Q490DRL2 steel used for large-thickness pressure vessels often exhibits fluctuations in transverse impact energy specifically manifested as significant variations in individual impact values. In this study, for Q490DRL2 steel with a thickness of 48 mm, specimens taken from the half-thickness position with superior and inferior impact energy were comparatively analyzed in terms of microstructural characteristics and inclusion distribution patterns. The results indicate that the matrix microstructures of the two types of specimens are essentially consistent. However, the fracture surface of the specimen with inferior impact energy exhibits a distinct serrated morphology, with numerous fine cracks present near the fracture surface. Some of these cracks pre-existed in the material, while others initiated and propagated during impact loading. Additionally, pronounced microstructural segregation and propagated large-sized cracks were observed in the matrix of this specimen, with fragmented square silicate inclusions visible inside the cracks. In contrast, the fracture surface of the specimen with superior impact energy is relatively flat and smooth, with few observable microcracks and a reduced presence of large inclusion particles in the matrix. In summary, large-particle silicate inclusions and microstructural segregation are the primary factors contributing to the fluctuation in low-temperature impact energy of Q490DRL2 steel used for large-thickness pressure vessels.  
      关键词:Pressure Vessel Steel;Impact Energy;Metallographic Microstructure;Inclusion   
      135
      |
      44
      |
      0
      <HTML>
      <L-PDF><WORD><Meta-XML>
      <引用本文> <批量引用> 156511362 false
      更新时间:2026-11-16
    • Luan Guoqing, Chen Guanghui, Qi Xiaotao, Liu Chao, Wan Xiangliang
      Vol. 47, Issue 6, Pages: 120-127(2026) DOI: 10.20057/j.1003-8620.N260098
      摘要:To overcome the key challenge that coarse austenite grains restrict the strength and ductility of high-C medium-Mn steels, the microstructure, mechanical properties, and fracture mechanism of an Fe-1.4C-8Mn-2Al high-C medium-Mn austenitic twinning-induced plasticity (TWIP) steel were systematically investigated. The effects of three processing routes, namely casting plus solution treatment, hot rolling plus solution treatment, and selective laser melting (SLM) additive manufacturing, on the microstructure and mechanical performance of the experimental steel were comparatively evaluated. The results demonstrated that the as-cast + solution-treated steel, characterized by severe austenite grain coarsening (approximately 1 mm), exhibited a yield strength of merely 371 MPa and an elongation of approximately 15%. Furthermore, stress serrations observed during tensile testing indicated premature fracture induced by internal or surface cracks. Following hot rolling and solution treatment, grain refinement to 370 μm increased the yield strength to 447 MPa and improved the elongation to 20%. Nevertheless, the grains remained relatively coarse. The SLM-processed steel achieved a yield strength of 687 MPa, attributed to grain refinement strengthening resulting from an ultrahigh cooling rate. However, the elongation decreased to 14%, with discontinuous regions observed on the fracture surface. The intergranular fracture observed in the as-cast + solution-treated and hot-rolled + solution-treated steels was closely associated with grain boundary stress concentration arising from coarse grains, as well as incompatible plastic deformation. The insufficient ductility of the SLM steel resulted from non-uniform grain size distributions, characterized by the coexistence of equiaxed grains and <100>-oriented columnar grains, as well as manufacturing defects. Future efforts should focus on optimizing SLM process parameters to suppress crystallographic preferred orientation and eliminate defects such as unmelted powder particles or shrinkage porosity. Furthermore, post-heat treatment can also be employed to optimize the compositional homogeneity and microstructural uniformity, thereby achieving an excellent combination of high strength and superior ductility.  
      关键词:High-C Medium-Mn Steel;Hot Rolling;Grain Size;TWIP Effect;Additive Manufacturing   
      50
      |
      63
      |
      0
      <HTML>
      <L-PDF><WORD><Meta-XML>
      <引用本文> <批量引用> 166634187 false
      更新时间:2026-11-16
    • Cheng Jun, Peng Kangwei, Wang Jing, Zhai Xinqi, Gong Bingli
      Vol. 47, Issue 6, Pages: 128-134(2026) DOI: 10.20057/j.1003-8620.N260026
      摘要:Laser polishing can effectively improve the surface quality of cold work die steel Cr12MoV. To explore the influencing factors of surface quality during laser polishing, an orthogonal experimental design was employed to formulate the experimental protocol. Cr12MoV die steel surfaces were treated using varying laser polishing parameters. Through characterization of the polished layer microstructure and geometric features such as cracks, the mechanisms underlying crack initiation and propagation during laser polishing of Cr12MoV die steel were examined. SPSS software was utilized to assess the influence patterns of laser polishing parameters on surface quality metrics of the polished regions, including remelted zone depth, polished layer depth, surface roughness, and crack formation. The results show that the surface roughness of all polished die steel specimens across experimental groups was reduced compared to the original surface, with the minimum value reaching 0.944 μm, decreased by 88.8% relative to the original surface. Crack formation was observed on the polished surfaces of die steel specimens in certain groups subjected to higher polishing power. During laser polishing of Cr12MoV die steel, laser process parameters directly effect surface quality indicators such as remelted zone depth, polished layer depth, crack dimensions, and surface roughness. Among these parameters, laser power and scanning speed are significant factors affecting the aforementioned surface quality metrics, whereas the influence of overlap rate is non-significant. Optimal selection of laser polishing process parameters can effectively enhance the surface quality of Cr12MoV die steel.  
      关键词:Cr12MoV;Laser polishing;Process Parameter;Cracking;Thermal effect   
      142
      |
      300
      |
      0
      <HTML>
      <L-PDF><WORD><Meta-XML>
      <引用本文> <批量引用> 153980088 false
      更新时间:2026-11-16
    0