Huang Yongzhi,Gao Zhiming,Lü Chuantao,et al.Research and Development of High-Performance Bimetallic Metallurgically Bonded Composite Tubing and Casing[J].Special Steel,2026,47(06):1-6.
Huang Yongzhi,Gao Zhiming,Lü Chuantao,et al.Research and Development of High-Performance Bimetallic Metallurgically Bonded Composite Tubing and Casing[J].Special Steel,2026,47(06):1-6.DOI:.
Research and Development of High-Performance Bimetallic Metallurgically Bonded Composite Tubing and Casing
Aiming at the bottleneck of severe corrosion failure of conventional casing and tubing
in the development of deep, ultra-deep and high-sour oil and gas fields in China, a systematic study on key technologies of high-performance bimetallic metallurgically bonded composite OCTG was carried out. By adopting an innovative material system of "high-strength sour-service low alloy steel outer layer + corrosion-resistant alloy (CRA) inner layer", the critical chemical composition ranges (mass fraction) of the outer sour-service low alloy steel ( ≤ 0.008%P, ≤ 0.002%S, 0.50%-1.00%Cr, 0.20%-0.40%Mo) and the main composition of the inner 20-40 type nickel-based CRA (20.00%-23.00% Cr, ≥40.00% Ni, 5.00%-8.00% Mo) were determined. A short-process manufacturing route combining "electroslag remelting (ESR) composite billet + controlled rolling and cooling" was developed, through which the key process parameters were established: ESR melting rate controlled at 5.0-6.5 kg/min, initial hot rolling temperature of 1 150-1 200 ℃, finish rolling temperature ≥ 900 ℃, cumulative reduction ≥ 60%, quenching temperature of 900-950 ℃, and tempering temperature of 600-680 ℃. For the
88.9 mm×7.34 mm composite pipe, the interfacial shear strength reached 572-585 MPa, and the tensile strength of the outer low alloy steel was 865-982 MPa. Under simulated harsh service conditions, the uniform corrosion rate was ≤ 0.003 mm/a, which was two orders of magnitude lower than the industry standard. This achievement has been demonstrated in engineering applications in highly corrosive oil and gas fields, providing technical support for the safe
and efficient development of deep oil and gas resources in China.
Carneiro R A , Ratnapuli R C , de Freitas Cunha Lins V . The influence of chemical composition and microstructure of API linepipe steels on hydrogen induced cracking and sulfide stress corrosion cracking [J]. Materials Science and Engineering: A , 2003 , 357 ( 1-2 ): 104 - 110 .
Baghaei M H , Faraji G . Punch plastic deformation pipe cladding (PPDPC) as a novel tube cladding method [J]. Journal of Advanced Materials and Processing , 2016 , 4 : 21 - 28 .
KleverR F J . On the mechanics of premium connections in casing and tubing [C]. SPE Annual Technical Conference and Exhibition. Society of Petroleum Engineers , 1992 . SPE-24692-MS.
API Speccificatio 5CT. Specification for casing and tubing [S]. 10 th ed. Washington : American Petroleum Institute , 2018 incorporating errata 3, 2020 .
NACE International . NACE TM0177-2016 laboratory testing of metals for resistance to sulfide stress cracking and stress corrosion cracking in H2S environments [S]. Houston : NACE International , 2016 .
Jiang Z , ZhangY , Wang L , et al . Corrosion behavior of stainless steel cladding layer in CO 2 -H 2 S-Cl⁻ environment [J]. Corrosion Science , 2021 , 187 : 109472 .
Wang H , Zhang Z , Chen S , et al . Advanced manufacturing technologies for corrosion resistant alloy-clad OCTG for extreme sour service [C]. SPE Annual Technical Conference and Exhibition , Houston, Texas, USA , October 3-5 , 2022 . SPE-200981.