It is available to produce high speed steel by rationally using abundant tungsten
molybdenum and vanadium ore resources in China and comprehensively applying high and advance technologies such as smelting reduction
electroslag remelting and microalloying so as to attain the goal economically utilizing these resources
increasing metallurgical quality
decreasing energy consumption
shortening process flow sheet and improving environment. In the meantime the production base to produce pit tool
die and cold-rolling roller of high speed steel according to international standards should be established to meet the steady increasing requirement of domestic manufacturing industry and to change resources export for products export in international market.