阴树标, 刘清友, 孙新军, et al. Effect of Hot Rolling Parameters on Deformation Resistance of Coarse-Grained Niobium Steel[J]. Special Steel, 2007, 28(2): 26-28.
阴树标, 刘清友, 孙新军, et al. Effect of Hot Rolling Parameters on Deformation Resistance of Coarse-Grained Niobium Steel[J]. Special Steel, 2007, 28(2): 26-28.DOI:
The deformation resistance of niobium steel 0. 05C
1. 44Mn
0. 13Nb with austenite grain size 800 μm during control rolling at 900 ~ 1 050 °C with deformation rate 1 ~ 20 s ~ and true strain 0 -0. 7 has been studied by Thermecomaster-Z thermal simulation test machine
and a regression equation for deformation resistance is established. Test results showed that with increasing temperature
deformation resistance of niobium steel in austenite region decreased
at same temperature with increasing straining
deformation resistance of steel increased
and at given straining deformation resistance increased with increasing deformation rate. The difference in deformation resistance between calculation value by regression equation and measured value was W5 MPa.