仇晓磊, 孟庆玉, 洪新. Math Simulation for Process Energy Consumption of Scrap-EAF Flow Sheet and Hot Metal+ Scrap-EAF Flow Sheet[J]. Special Steel, 2007, 28(3): 4-6.
仇晓磊, 孟庆玉, 洪新. Math Simulation for Process Energy Consumption of Scrap-EAF Flow Sheet and Hot Metal+ Scrap-EAF Flow Sheet[J]. Special Steel, 2007, 28(3): 4-6.DOI:
Based on materials balance model and heat balance model and combined with relative process parameters
the calculated models for process energy consumption of scrap-arc fumace steelmaking-concasting-continuous rolling(scrap- EAF)flow sheet and hot metal +scrap-arc fumace-concasting-continuous rolling(metal+ scrap-EAF)flow sheet have been established and the effect of several key parameters on process energy consumption is analyzed. Results showed that compared with scrap-EAF flow sheet the process energy consumption of 33% metal+ scrap-EAF increased by 43.72 kg
ce
/t
stsel
but its total energy consumption of flow sheet increased by 1/3.